Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.308 GPa @Strain 9.80 %, Temperature 100 °C |
44.7 ksi @Strain 9.80 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |