Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 5.04 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.04 GPa

@Strain 1.02 %,
Temperature 23.0 °C
731 ksi

@Strain 1.02 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.04 GPa

@Strain 1.02 %,
Temperature 23.0 °C
731 ksi

@Strain 1.02 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.04 GPa

@Strain 1.67 %,
Temperature 0.000 °C
731 ksi

@Strain 1.67 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Secant Modulus 5.04 GPa

@Strain 1.12 %,
Temperature 40.0 °C
731 ksi

@Strain 1.12 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Secant Modulus 5.04 GPa

@Strain 1.99815 %,
Temperature 40.0 °C
731 ksi

@Strain 1.99815 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..