Polymer Property : Secant Modulus = 5.456 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.456 GPa

@Strain 2.50 %,
Temperature -20.0 °C
791.3 ksi

@Strain 2.50 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..