Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.84 GPa @Strain 1.60 %, Temperature 100 °C |
558 ksi @Strain 1.60 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |