Polymer Property : Secant Modulus = 57.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.393 GPa

@Strain 9.00 %,
Temperature 80.0 °C
57.0 ksi

@Strain 9.00 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub..
Secant Modulus 0.393 GPa

@Strain 9.00 %,
Temperature 80.0 °C
57.0 ksi

@Strain 9.00 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing ..
Secant Modulus 0.393 GPa

@Strain 5.34 %,
Temperature 40.0 °C
57.0 ksi

@Strain 5.34 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers