Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.04857 - 6.80 GPa @Temperature -40.0 - 100 °C |
152.085 - 986 ksi @Temperature -40.0 - 212 °F |
Average value: 3.63 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Secant Modulus | 1.04857 - 6.80 GPa @Strain 0.250 - 3.50 % |
152.085 - 986 ksi @Strain 0.250 - 3.50 % |
Average value: 3.63 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |