Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.7735 GPa @Strain 2.00 %, Temperature 40.0 °C |
692.35 ksi @Strain 2.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |