Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.66 GPa @Strain 0.320 %, Temperature 40.0 °C |
1110 ksi @Strain 0.320 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |