Polymer Property : Secant Modulus = 782 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.39 GPa

@Strain 1.77 %,
Temperature 40.0 °C
782 ksi

@Strain 1.77 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Secant Modulus 5.39 GPa

@Strain 2.00 %,
Temperature -40.0 °C
782 ksi

@Strain 2.00 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..