Mechanical Properties Metric English Comments
Secant Modulus 9.10 GPa

@Strain 1.33 %,
Temperature -20.0 °C
1320 ksi

@Strain 1.33 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Secant Modulus 9.10 GPa

@Strain 1.33 %,
Temperature -20.0 °C
1320 ksi

@Strain 1.33 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Secant Modulus 9.10 GPa

@Strain 2.20 %,
Temperature 23.0 °C
1320 ksi

@Strain 2.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..