Polymer Property : Secant Modulus = 9.37 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 9.37 GPa

@Strain 1.10 %,
Temperature 0.000 °C
1360 ksi

@Strain 1.10 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Secant Modulus 9.37 GPa

@Strain 0.100 %,
Temperature 100 °C
1360 ksi

@Strain 0.100 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**)
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers