Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 3.70 J @Load <=102 kg, Temperature 23.0 °C |
2.73 ft-lb @Load <=225 lb, Temperature 73.4 °F |
d.a.m.; ISO 6603-2 |
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Puncture Energy | 3.70 J @Load <=133 kg, Temperature -30.0 °C |
2.73 ft-lb @Load <=292 lb, Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS. |