Mechanical Properties Metric English Comments
Puncture Energy 59.0 J

@Temperature 23.0 °C
43.5 ft-lb

@Temperature 73.4 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan EX401 Copolyester
Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are..
Puncture Energy 59.0 J

@Temperature 23.0 °C
43.5 ft-lb

@Temperature 73.4 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan LX201 Copolyester
Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are..