Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 2.40 J/cm²
11.4 ft-lb/in²
ISO 180
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..