Mechanical Properties Metric English Comments
Izod Impact Resistance 2.67 J/cm²
12.7 ft-lb/in²
Dow DOWLEX™ IP-41 High Density Polyethylene
DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpo..
Izod Impact Resistance 2.67 J/cm²
12.7 ft-lb/in²
Dow HDPE 38152M High Density Polyethylene
DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent proces..