Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dynatup @ -30°C 61.0 J

@Thickness 3.17 mm
45.0 ft-lb

@Thickness 0.125 in
ARM Std. Low Temp Impact; ARM Std.
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements..
Dynatup @ -30°C 61.0 J

@Thickness 3.17 mm
45.0 ft-lb

@Thickness 0.125 in
ARM Std. Low Temp Impact; ARM Std.
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec..
Dynatup @ -30°C 61.0 J

@Thickness 3.17 mm
45.0 ft-lb

@Thickness 0.125 in
ARM Std. Low Temp Impact; ARM Std.
Formosa Plastics Formolene® L63565U Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63565U is fully heat and UV stabilized.Meets all requirement..
Dynatup @ -30°C 61.0 - 81.3 J
45.0 - 60.0 ft-lb
Average value: 71.2 J Grade Count:6
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report..
Copyright © lookpolymers.com All Rights Reserved