Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® L63550U Rotational Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® L63550U Rotational Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 300 hour
300 hour
Condition A (10% Igepal), F<sub>50</sub>; ASTM D1693
>= 1000 hour
>= 1000 hour
Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.6 MPa
2700 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 11.8 %
11.8 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
1.3mm per min; ASTM D790
Dynatup @ -30°C 61.0 J

@Thickness 3.17 mm
45.0 ft-lb

@Thickness 0.125 in
ARM Std. Low Temp Impact; ARM Std.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648