Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
200% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
200% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
200% Modulus | 0.00520 GPa | 0.754 ksi | ASTM D412 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
200% Modulus | 0.00520 GPa | 0.754 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Low Cost General Purpose Hose FormulationNordel® IP 4640 |