Polymer Property : 200% Modulus = 0.0331 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.0331 GPa
4.80 ksi
ASTM D412
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane
Type: Estane® ALR E68D-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp..