Mechanical Properties Metric English Comments
200% Modulus 0.00293 GPa
0.425 ksi
ASTM D412-92
Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation
Description: Versilicâ„¢ SPX-50: Peroxide-cured Versilicâ„¢ High-Strength Silicone Tubing is designed for use in applications where flexibility, resiliency and durability are required. Its s..