Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation

Category Polymer , Thermoset , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Versilic™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Versilic™ SPX-50: Peroxide-cured Versilic™ High-Strength Silicone Tubing is designed for use in applications where flexibility, resiliency and durability are required. Its smooth inner surface reduces the risk of particulate entrapment and microscopic buildup during fluid transfer. In addition, its high and low working temperatures help the tubing retain its flexibility under extreme conditions. Because of its consistently reliable performance, Versilic™ High-Strength Silicone Tubing is ideal for applications such as food & beverage dispensing & processing, appliance manufacturing, cosmetic production and electronic equipment. Custom formulations can be designed to provide a combination of features, including ultra-high temperature resistance, electrical conductivity, pigmented colors and long flexural life. Features/Benefits:Provides resiliency, long life and durabilityUltra-smooth inner bore reduces risk of particulate entrapmentExcellent Pressure CapabilitiesTaste and odor freeWithstands temperature extremes from -75°F to 350°FMeets FDA, 3-A ad NSF criteriaTypical applications include Veterinary Pharmaceuticals, Respiratory and Anesthesia Equipment, Sterile Filling and Processing, Analytical Instrumentation, Cosmetic Production, Environmental Remediation, Beverage Dispensing, Food and Dairy Processing, Appliance Manufacturing, Electronic EquipmentInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792-91
Water Absorption 0.060 %
0.060 %
24 hours at 23°C; ASTM D570-81
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
15 seconds; ASTM D2240-91
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D412-92
Elongation at Break 450 %
450 %
ASTM D412-92
200% Modulus 0.00293 GPa
0.425 ksi
ASTM D412-92
Tear Strength 25.9 kN/m
148 pli
Initial Tear Strength; ASTM D624-91 Die B
Compression Set 10 %

@Temperature 70.0 °C
10 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
33 %

@Temperature 175 °C
33 %

@Temperature 347 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
204 °C
400 °F
Intermittent
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746-79
Electrical Properties Metric English Comments
Dielectric Strength 18.9 kV/mm
480 kV/in
ASTM D149-93
Descriptive Properties Value Comments
Color Translucent