Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 53.4 J/cm | 0.100 ft-lb/mil | 23°C, C.125 Tup, Method A; ASTM D-4226 |
Axiall 7181 Rigid PVC, Extrusion Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret.. |