Polymer Property : Gardner Impact = 0.450 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 0.450 J
0.332 ft-lb
J; ASTM D3029-GB, unpainted
Plaskolite Optix® Acrylic Sheet
Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,..
Gardner Impact 0.450 - 5.30 J
0.332 - 3.91 ft-lb
Average value: 2.49 J Grade Count:4
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..