Gardner Impact 0.450 - 5.30 J
0.332 - 3.91 ft-lb
Average value: 2.49 J Grade Count:4
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..