Polymer Property : Gardner Impact = 0.516 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene
PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.Data provided by Multibase.
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 2005 T BLK Polypropylene
PP compound suitable for automotive applications, meets elevated temperature resistance. Meets ESH-M4D-293-B specifications.Data provided by Multibase.
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 4006 T H BLK 40% Talc Content Polypropylene
Multi-Pro 4002 T H is a talc reinforced polypropylene compound with excellent stiffness at medium impact resistance. Its heat resistance is improved over natural and can resist 150°C for 750 hours..
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D3029
Adell EA-14 Homopolymer Polypropylene, 20% Talc Filled
Data provided by Adell Plastics, Inc.
Gardner Impact 0.700 J
0.516 ft-lb
ASTM D3029
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.