Polymer Property : Gardner Impact = 1.667 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D3029
Multibase Nylex™ 2112 FR V0 Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D3029
Multibase Nylex™ 2185 CR Polyamide + PP
Forms: PelletsFeatures:Chemical Resistance, GoodInformation provided by Multibase
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D3029
Multibase Nylex™ 2185 HFX Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D5420
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D3029
Multibase Multi-Flam™ 0106 PP Black Polypropylene
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase