Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM 792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ASTM D955
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.6 MPa
5750 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Gardner Impact 2.260 J
1.667 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
0.125 in