Mechanical Properties Metric English Comments
Gardner Impact 2.30 J
1.70 ft-lb
ASTM D3029
Washington Penn PPH2UFO Polypropylene, Unfilled
Homopolymer for injection molding. Meets General Motors spec. GMP.PP.013Data provided by Washington Penn Plastic Co., Inc.
Gardner Impact 2.30 J
1.70 ft-lb
ASTM D3029
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled
Data provided by Adell Plastics, Inc.