Adell RA-16 Copolymer Polypropylene, 30% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RA-16 Copolymer Polypropylene, 30% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 49
49
ASTM D785
Hardness, Rockwell R 76
76
ASTM D785
Tensile Strength, Ultimate 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.70 J/cm
6.93 ft-lb/in
ASTM D256
Gardner Impact 2.30 J
1.70 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: