Mechanical Properties Metric English Comments
Gardner Impact >= 21.7 J

@Thickness 3.17 mm
>= 16.0 ft-lb

@Thickness 0.125 in
ASTM D5420
S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant
Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers
Gardner Impact 21.7 J

@Temperature 22.8 °C
16.0 ft-lb

@Temperature 73.0 °F
ASTM D5420
Spartech PP5230 Calcium Carbonate Filled Homopolymer
Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal..
Gardner Impact 21.7 J

@Temperature 22.8 °C
16.0 ft-lb

@Temperature 73.0 °F
ASTM D5420
Spartech PP7130 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Gardner Impact 21.7 J
16.0 ft-lb
ASTM D5420
Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
Gardner Impact 21.7 J

@Temperature 23.0 °C
16.0 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 62 mil
Axiall CL-7049 Rigid PVC, Molding
Georgia Gulf CL-7049 is a clear, high impact vinyl compound formulated for medical and food contact uses.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Gardner Impact 21.7 J

@Temperature 23.0 °C
16.0 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 62 mil
Axiall CL-7053 Rigid PVC, Molding
Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.