Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Teknor Apex Company
Trade Name Synres®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many other applications requiring high rigidity. These compounds can be tailored to specific needs and are available pre-colored or natural. Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ash 20 %
20 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
10 seconds; ASTM D2240
Tensile Strength at Break 64.5 MPa

@Thickness 50.8 mm
9350 psi

@Thickness 2.00 in
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Gardner Impact 21.7 J
16.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
314 °F
ASTM D648B