Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Multibase Multi-Flex® TPE D 4510 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-187 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9779 Medium Grey Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-501UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 149B Shale Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J @Temperature -18.0 °C |
16.7 ft-lb @Temperature -0.400 °F |
|
Network Polymers NPP 25-1002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR7 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 260F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
Method G, geometry GC; ASTM D5420 |
Pinnacle Polymers 3208 High Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J @Thickness 3.17 mm |
16.7 ft-lb @Thickness 0.125 in |
ASTM D3029 |
Ineos Styrenics Polystyrene 476M (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Gardner Impact | 22.6 J @Temperature 23.0 °C |
16.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 67 mil |
Axiall MP-6510 Rigid PVC, Molding Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a.. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products E204-00 High Density Polyethylene, Natural Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-FR7 Modified PPO, V-0 Flame Retardant, Medium Heat, 250 HDT
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |