Mechanical Properties Metric English Comments
Gardner Impact 19.0 J

@Temperature -30.0 °C
14.0 ft-lb

@Temperature -22.0 °F
ASTM D3029
LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplication..
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..
Gardner Impact 19.0 J

@Temperature 23.0 °C
14.0 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Medium Impact Copolymer 50% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..
Gardner Impact 19.0 J
14.0 ft-lb
ASTM D3029
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene
DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided ..