Polymer Property : Gardner Impact = 2.00 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
Flint Hills P4G2T-077D Homopolymer Polypropylene
Homopolymer, FDA compliantFeatures: Antistat.Applications: Extrusion: straw grade.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Gardner Impact 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills P4G4A-053 Polypropylene Homopolymer
Features: Good stiffness, long term heat aging (LTHA). Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: High heat resistanceInformation Provided ..
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
Flint Hills P4G4Z-011 Homopolymer Polypropylene
Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: Applications: Injection molding: general purpose, extruded decorative ribbon, and extruded fiber.Former Huntsman polypr..
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D5420
Flint Hills P5C6Z-075 Random Copolymer Polypropylene
Features: Phthalate-free.Applications: Fibers, BCF, SpunbondedInformation provided by Flint Hills Resources.
Gardner Impact 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills P9G8Z-036 Polypropylene Specialty Polypropylene
Features: Broad MWD Homopolymer. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion coatingInformation Provided by Flint Hills Resources
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
Flint Hills P9H8M-015 Polypropylene
Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D5420
Flint Hills P9H8M-058X Specialty Polypropylene
Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro..
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant
Key Features: medium high melt flow, medium high modulus, flame retardant, low specific gravity, good impact strengthApplications: battery jars, electrical componentsDescription: Astryn BA905-74 med..
Gardner Impact 2.00 J

@Temperature -30.0 °C
1.47 ft-lb

@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer
Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil..
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled
Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag..
Gardner Impact 2.00 J
1.48 ft-lb
Geometry GB; ASTM D5420
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma..