Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 10.0 - 20.0 J | 7.38 - 14.8 ft-lb | SABIC Method |
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East) NORYL FN150 twin wall foam meets UL standard 94 V-0/5V ratings at 4 mm wall thickness. These unique flammability characteristics make FN150 the supreme choice for designing optimum wall thickness in.. |