Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 10.0 J @Temperature 23.0 °C |
7.38 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Flint Hills P4C4T-189 Polypropylene Homopolymer Features: Visbroken, Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: ClosuresInformation Provided by Flint Hills Resources |
|||
Gardner Impact | 10.0 J @Temperature 23.0 °C |
7.38 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Noryl BN30 PPE+PS Blowmoldable. DTUL 180F. UL rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Gardner Impact | 10.0 - 20.0 J | 7.38 - 14.8 ft-lb | SABIC Method |
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East) NORYL FN150 twin wall foam meets UL standard 94 V-0/5V ratings at 4 mm wall thickness. These unique flammability characteristics make FN150 the supreme choice for designing optimum wall thickness in.. |