Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 43.0 - 54.0 J | 31.7 - 39.8 ft-lb | Average value: 48.5 J Grade Count:5 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357U PBT+PC Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Gardner Impact | 43.0 J | 31.7 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Valox® 357U PBT+PC Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |