Polymer Property : Gardner Impact = 54.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 43.0 - 54.0 J
31.7 - 39.8 ft-lb
Average value: 48.5 J Grade Count:5
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..