Polymer Property : Gardner Impact = 4.13 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 5.60 J
4.13 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene
Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex..