Mechanical Properties Metric English Comments
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 215HPR PBT
Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21..
Gardner Impact 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Valox® 295 PBT
Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 310HP PBT
PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 311 PBT
Unreinforced, improved resistance to UV. Medium viscosity.
Gardner Impact 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Valox® 312 PBT
Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific)
Unreinforced, For compounding only (not for injection molding), Medium viscosity.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 315 PBT
Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
Gardner Impact 40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Valox® 325M PBT (Asia Pacific)
325M is a high flow VALOX 325 for restrictive gate tooling (key buttons)This data was supplied by SABIC-IP for the Asia Pacific region.