SABIC Innovative Plastics Valox® 215HPR PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® 215HPR PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX215HP.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Viscosity 100000 cP
100000 cP
Melt Viscosity; SABIC Method
Linear Mold Shrinkage, Flow 0.0090 - 0.016 cm/cm

@Thickness 0.750 - 2.30 mm
0.0090 - 0.016 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
0.015 - 0.023 cm/cm

@Thickness 2.30 - 4.60 mm
0.015 - 0.023 in/in

@Thickness 0.0906 - 0.181 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm

@Thickness 0.750 - 2.30 mm
0.010 - 0.017 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
0.016 - 0.024 cm/cm

@Thickness 2.30 - 4.60 mm
0.016 - 0.024 in/in

@Thickness 0.0906 - 0.181 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 10 %
10 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 82.0 MPa
11900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 16.02 J/cm
30.01 ft-lb/in
ASTM D4812
Gardner Impact 40.0 J
29.5 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 154 °C

@Thickness 6.40 mm
309 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C

@Thickness 6.40 mm
129 °F

@Thickness 0.252 in
unannealed; ASTM D648
Descriptive Properties Value Comments
Specific Volume 0.76cm^3/g
ASTM D792