Mechanical Properties Metric English Comments
Gardner Impact 0.678 - 10.2 J
0.500 - 7.52 ft-lb
Average value: 5.93 J Grade Count:4
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..