This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.905 - 3.15 g/cc
0.0327 - 0.114 lb/in³
Average value: 1.19 g/cc Grade Count:247
Filler Content 10.0 - 75.0 %
10.0 - 75.0 %
Average value: 43.5 % Grade Count:22
Maximum Moisture Content 0.0100
0.0100
Average value: 0.0100 Grade Count:19
Linear Mold Shrinkage 0.000900 - 0.0600 cm/cm
0.000900 - 0.0600 in/in
Average value: 0.00964 cm/cm Grade Count:177
Linear Mold Shrinkage, Transverse 0.00460 - 0.0170 cm/cm
0.00460 - 0.0170 in/in
Average value: 0.0117 cm/cm Grade Count:29
Melt Flow 0.500 - 100 g/10 min
0.500 - 100 g/10 min
Average value: 15.2 g/10 min Grade Count:223
Ash 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 25.0 % Grade Count:40
Mechanical Properties Metric English Comments
Hardness, Rockwell R 43.0 - 100
43.0 - 100
Average value: 77.7 Grade Count:53
Hardness, Shore D 55.0 - 78.0
55.0 - 78.0
Average value: 71.3 Grade Count:24
Ball Indentation Hardness 23.0 - 90.0 MPa
3340 - 13100 psi
Average value: 49.3 MPa Grade Count:31
Tensile Strength, Ultimate 10.0 - 65.0 MPa
1450 - 9430 psi
Average value: 23.8 MPa Grade Count:133
7.00 - 16.0 MPa

@Temperature 60.0 - 120 °C
1020 - 2320 psi

@Temperature 140 - 248 °F
Average value: 11.4 MPa Grade Count:4
Tensile Strength, Yield 10.0 - 85.3 MPa
1450 - 12400 psi
Average value: 26.8 MPa Grade Count:173
Elongation at Break 1.60 - 500 %
1.60 - 500 %
Average value: 44.6 % Grade Count:174
6.00 - 35.0 %

@Temperature 60.0 - 90.0 °C
6.00 - 35.0 %

@Temperature 140 - 194 °F
Average value: 58.3 % Grade Count:5
Elongation at Yield 2.00 - 100 %
2.00 - 100 %
Average value: 8.83 % Grade Count:114
3.40 - 10.0 %

@Temperature 60.0 - 90.0 °C
3.40 - 10.0 %

@Temperature 140 - 194 °F
Average value: 6.61 % Grade Count:5
Modulus of Elasticity 0.950 - 5.40 GPa
138 - 783 ksi
Average value: 2.41 GPa Grade Count:147
0.500 - 4.90 GPa

@Temperature 60.0 - 90.0 °C
72.5 - 711 ksi

@Temperature 140 - 194 °F
Average value: 1.37 GPa Grade Count:5
Flexural Yield Strength 14.0 - 127 MPa
2030 - 18500 psi
Average value: 38.4 MPa Grade Count:143
Flexural Modulus 0.239 - 9.00 GPa
34.7 - 1310 ksi
Average value: 2.42 GPa Grade Count:208
0.560 - 1.25 GPa

@Temperature 60.0 - 120 °C
81.2 - 181 ksi

@Temperature 140 - 248 °F
Average value: 0.893 GPa Grade Count:1
Izod Impact, Notched 0.200 - 100 J/cm
0.375 - 187 ft-lb/in
Average value: 0.620 J/cm Grade Count:119
0.150 - 10.0 J/cm

@Temperature -40.0 - 0.000 °C
0.281 - 18.7 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.495 J/cm Grade Count:13
0.196133 - 0.220 J/cm

@Temperature -30.0 - -10.0 °C
0.367438 - 0.412 ft-lb/in

@Temperature -22.0 - 14.0 °F
Average value: 0.495 J/cm Grade Count:10
0.196133 - 0.220 J/cm

@Thickness 3.20 - 6.40 mm
0.367438 - 0.412 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.495 J/cm Grade Count:10
Izod Impact, Unnotched 1.33 J/cm - NB
2.49 ft-lb/in - NB
Average value: 5.36 J/cm Grade Count:8
1.0678 - 1.0678 J/cm

@Temperature -18.0 - -18.0 °C
2.0004 - 2.0004 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 1.07 J/cm Grade Count:1
Izod Impact, Notched (ISO) 2.00 - 57.0 kJ/m²
0.952 - 27.1 ft-lb/in²
Average value: 17.5 kJ/m² Grade Count:63
1.70 - 43.0 kJ/m²

@Temperature -40.0 - 10.0 °C
0.809 - 20.5 ft-lb/in²

@Temperature -40.0 - 50.0 °F
Average value: 5.81 kJ/m² Grade Count:31
Izod Impact, Unnotched (ISO) 15.0 kJ/m² - NB
7.14 ft-lb/in² - NB
Average value: 59.7 kJ/m² Grade Count:9
21.0 - 200 kJ/m²

@Temperature -20.0 - -20.0 °C
9.99 - 95.2 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 72.5 kJ/m² Grade Count:4
Charpy Impact Unnotched 0.700 J/cm² - NB
3.33 ft-lb/in² - NB
Average value: 4.68 J/cm² Grade Count:87
0.500 J/cm² - NB

@Temperature -40.0 - -20.0 °C
2.38 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 4.14 J/cm² Grade Count:56
Charpy Impact, Notched 0.150 - 7.00 J/cm²
0.714 - 33.3 ft-lb/in²
Average value: 1.46 J/cm² Grade Count:100
0.0300 - 2.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.143 - 9.52 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.413 J/cm² Grade Count:58
Gardner Impact 0.678 - 10.2 J
0.500 - 7.52 ft-lb
Average value: 5.93 J Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 30.0 - 140 µm/m-°C
16.7 - 77.8 µin/in-°F
Average value: 63.7 µm/m-°C Grade Count:20
Melting Point 160 - 168 °C
320 - 334 °F
Average value: 164 °C Grade Count:47
Maximum Service Temperature, Air 75.0 - 140 °C
167 - 284 °F
Average value: 111 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 72.0 - 156 °C
162 - 313 °F
Average value: 115 °C Grade Count:165
Deflection Temperature at 1.8 MPa (264 psi) 44.0 - 150 °C
111 - 302 °F
Average value: 69.7 °C Grade Count:192
Vicat Softening Point 36.0 - 161 °C
96.8 - 322 °F
Average value: 111 °C Grade Count:110
UL RTI, Electrical 65.0 - 120 °C
149 - 248 °F
Average value: 76.0 °C Grade Count:9
UL RTI, Mechanical with Impact 65.0 - 120 °C
149 - 248 °F
Average value: 76.0 °C Grade Count:9
UL RTI, Mechanical without Impact 65.0 - 120 °C
149 - 248 °F
Average value: 76.0 °C Grade Count:9
Flammability, UL94 HB - 5VB
HB - 5VB
Grade Count:72
Flame Spread 22.0 - 22.1 mm/min
0.866 - 0.870 in/min
Average value: 22.1 mm/min Grade Count:4
Oxygen Index 22.0 - 29.0 %
22.0 - 29.0 %
Average value: 25.6 % Grade Count:14
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
Average value: 7.50e+14 ohm-cm Grade Count:22
Surface Resistance 3000 - 1.00e+15 ohm
3000 - 1.00e+15 ohm
Average value: 1.35e+14 ohm Grade Count:23
Dielectric Strength 24.0 - 43.0 kV/mm
610 - 1090 kV/in
Average value: 41.1 kV/mm Grade Count:11
Comparative Tracking Index 400 - 600 V
400 - 600 V
Average value: 589 V Grade Count:27