Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 10.0 - 20.0 J @Temperature -20.0 °C |
7.38 - 14.8 ft-lb @Temperature -4.00 °F |
Longitudinal |
Bisalloy Steels BisPlate HHA Thickness 5-25 mm A quenched and tempered steel armor plate suitable for use in both military and civil applications where light weight and resistance to ballistic projectiles is required. |