Polymer Property : Charpy Impact = 20.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.7 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 4.8 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 3.2 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Charpy Impact 20.0 J

@Temperature -40.0 °C
14.8 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp XABO® 500 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 20.0 J

@Temperature -20.0 °C
14.8 ft-lb

@Temperature -4.00 °F
Transverse
ThyssenKrupp XABO® 500 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 20.0 J

@Temperature 538 - 816 °C
14.8 ft-lb

@Temperature 1000 - 1500 °F
Longitudinal
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..