Mechanical Properties Metric English Comments
Charpy Impact >= 40.7 J

@Treatment Temp. 579.4 °C,
Time 14400 sec
>= 30.0 ft-lb

@Treatment Temp. 1075 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Charpy Impact >= 40.7 J

@Treatment Temp. 621 °C,
Time 14400 sec
>= 30.0 ft-lb

@Treatment Temp. 1150 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Charpy Impact 40.7 J

@Temperature 538 °C
30.0 ft-lb

@Temperature 1000 °F
38-40 HRC; V-notch
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19
Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance..
Charpy Impact 40.7 J

@Tempering Temp. 510 °C
30.0 ft-lb

@Tempering Temp. 950 °F
oil quenched from 1525°F then tempered
Crucible Steel Holder Block Steel, AISI 4150 Modified
Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b..
Charpy Impact 40.7 J

@Tempering Temp. 204 °C
30.0 ft-lb

@Tempering Temp. 400 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel KETOS® Tool Steel, AISI O1
Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording..
Charpy Impact 40.7 J

@Tempering Temp. 260 °C
30.0 ft-lb

@Tempering Temp. 500 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel KETOS® Tool Steel, AISI O1
Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording..