Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Steel Holder Block Steel, AISI 4150 Modified

Category Metal , Ferrous Metal , Alloy Steel , AISI 4000 Series Steel
Manufacturer Crucible Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel Holder Block Steel, AISI 4150 Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also be used for light cold forming tools such as brake dies.Information provided by Crucible Industries
Physical Properties Metric English Comments
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 30

@Tempering Temp. 649 °C
30

@Tempering Temp. 1200 °F
oil quenched from 1525°F then tempered
36

@Tempering Temp. 538 °C
36

@Tempering Temp. 1000 °F
oil quenched from 1525°F then tempered
45

@Tempering Temp. 427 °C
45

@Tempering Temp. 800 °F
oil quenched from 1525°F then tempered
53

@Tempering Temp. 316 °C
53

@Tempering Temp. 600 °F
oil quenched from 1525°F then tempered
56

@Tempering Temp. 204 °C
56

@Tempering Temp. 400 °F
oil quenched from 1525°F then tempered
Modulus of Elasticity 200 GPa
29000 ksi
Charpy Impact 40.7 J

@Tempering Temp. 510 °C
30.0 ft-lb

@Tempering Temp. 950 °F
oil quenched from 1525°F then tempered
67.8 J

@Tempering Temp. 593 °C
50.0 ft-lb

@Tempering Temp. 1100 °F
oil quenched from 1525°F then tempered
74.6 J

@Tempering Temp. 649 °C
55.0 ft-lb

@Tempering Temp. 1200 °F
oil quenched from 1525°F then tempered
94.9 J

@Tempering Temp. 704 °C
70.0 ft-lb

@Tempering Temp. 1300 °F
oil quenched from 1525°F then tempered
Thermal Properties Metric English Comments
CTE, linear 11.7 µm/m-°C

@Temperature 21.1 - 93.3 °C
6.50 µin/in-°F

@Temperature 70.0 - 200 °F
12.6 µm/m-°C

@Temperature 21.1 - 204 °C
7.00 µin/in-°F

@Temperature 70.0 - 400 °F
Thermal Conductivity 3.31 W/m-K

@Temperature 93.3 °C
23.0 BTU-in/hr-ft²-°F

@Temperature 200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.50 %
0.50 %
Chromium, Cr 0.65 %
0.65 %
Iron, Fe 97 %
97 %
as balance
Manganese, Mn 1.25 %
1.25 %
Molybdenum, Mo 0.18 %
0.18 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.080 %
0.080 %
Users viewing this material also viewed the following: