Mechanical Properties Metric English Comments
Charpy Impact >= 74.6 J

@Treatment Temp. 760 °C,
Time 7200 sec
>= 55.0 ft-lb

@Treatment Temp. 1400 °F,
Time 2.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Charpy Impact >= 74.6 J

@Treatment Temp. 621 °C,
Time 14400 sec
>= 55.0 ft-lb

@Treatment Temp. 1150 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Charpy Impact 74.6 J

@Temperature 300 °C
55.0 ft-lb

@Temperature 572 °F
Longitudinal Charpy V-notch Tests from a 3" rolled plate at 293 HB
EDRO P1FM #31 Free Machining Holder Steel
EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis..
Charpy Impact 74.6 J

@Treatment Temp. 982 °C
55.0 ft-lb

@Treatment Temp. 1800 °F
austenitized; C-notch
Crucible Steel CPM® 4V® Tool Steel
CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blank..
Charpy Impact 74.6 J

@Treatment Temp. 593 °C
55.0 ft-lb

@Treatment Temp. 1100 °F
hardened H1100; V-notch
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel
CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm..
Charpy Impact 74.6 J

@Tempering Temp. 649 °C
55.0 ft-lb

@Tempering Temp. 1200 °F
oil quenched from 1525°F then tempered
Crucible Steel Holder Block Steel, AISI 4150 Modified
Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b..
Charpy Impact 74.6 J

@Temperature 499 °C
55.0 ft-lb

@Temperature 930 °F
V-notch (hardness of 45 HRC)
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o..
Charpy Impact 74.6 J

@Temperature 499 °C
55.0 ft-lb

@Temperature 930 °F
V-notch (hardness of 45 HRC)
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o..