Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 60.0 J @Temperature 0.000 °C |
44.3 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 60.0 J @Temperature 0.000 °C |
44.3 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 60.0 J @Temperature 0.000 °C |
44.3 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 60.0 J @Temperature 0.000 °C |
44.3 ft-lb @Temperature 32.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |