Polymer Property : Film Tensile Strength at Yield, MD = 8850 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 61.0 MPa

@Temperature 23.0 °C
8850 psi

@Temperature 73.4 °F
3% yield point. Orientation not specified; ASTM D882-91
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme..